Lithographic Method and Method for Testing a Lithographic Apparatus
FIELD
The present invention relates to a lithographic method.
BACKGROUND A lithographic apparatus is a machine that applies a desired pattern to a target portion or a substrate. Lithographic apparatus can be used, for example, in the manufacture of integrated circuits (ICs). In that circumstance, a patterning device, which is alternatively referred to as a mask or a reticle, may be used to generate a circuit pattern corresponding to an individual layer of the IC, and this pattern can be imaged onto a target portion (eg included part of, one or several dies) on a substrate (eg a silicon wafer) that has a layer of radiation-sensitive material (resist). In general, a single substrate will contain a network of adjacent target portions that are successively exposed. Known lithographic apparatus include so-called steppers, in which each target portion is irradiated by exposing an entire pattern onto the target portion in one go, and so-called scanners, in which each target portion is irradiated by scanning the pattern through the beam in a given direction (the "scanning" direction) while synchronously scanning the substrate parallel or anti-parallel to this direction.
There is a continuing desire to be able to generate patterns with finer resolution. In general, shorter wavelength radiation may be used in order to achieve a finer resolution pattern.
One method for providing patterns with increased resolution is dual trench patterning where a first pattern of trenches in a hardmask is overlapped by a second interleaved pattern of trenches in the hardmask to provide a final pattern in the hardmask or higher resolution than either the first or second patterns, which is then transferred to a target layer. Figures la to lj show schematically a dual trench patterning method for providing a high resolution pattern. Figure 1 shows in cross-section a portion of a silicon substrate 2 provided with a target layer 4 or polysilicon material. A hardmask layer 6 is provided on the target layer 4. A first layer of bottom anti-reflective coating (BARC) material 8 is provided on the hardmask layer 6 and a first layer of photoresist 10 is provided on the first layer of BARC material 8 The hardmask layer 6 is typically formed from an oxide material, such as S1O2 or SiON. The photoresist 10 may be any appropriate type or photoresist, such as, but not limited to, positive tone photoresist. A lithographic apparatus, which may be an example of the type shown schematically in Figure 3, is used to expose a pattern in the photoresist 10. The exposed photoresist 10 is then removed using a developer, such as a caustic solution containing hydroxide ions, so that only unexposed photoresist 10 remains. The pattern is then transferred to the BARC material 8 using an appropriate etching process, such as an ion etch.
The resulting structure, shown in Figure lb, comprises four lines 12 which extend perpendicularly to the plane of Figure lb. The full width of each line 12 is three times the width of the space 14 between each pair of lines 12. Only four lines 12 are shown, but it will be appreciated that Figure lb shows only a portion of the substrate 2, and that many more lines 12 may be provided on the substrate 2.
Referring to Figure 1c, the pattern formed in the photoresist 10 and BARC layer 8 is transferred to the hardmask layer 6 using a conventional hardmask etching process, such as an ion etch process. Referring to Figure Id, the first patterned BARC layer 8 and photoresist layer 10 are removed and then second layers of BARC 8a and photoresist 10a are provided on the patterned hardmask layer 6 as shown in Figure le. A different pattern is then formed in the second layers of BARC 8a and photoresist 10a such portions of the existing patterned hardmask 6 are uncovered, as shown in Figure 1 f. These uncovered portions of the hardmask 6 are then removed by a conventional etch process to yield the structure shown in Figure 1 g.
With reference to Figure lh, the second BARC 8a and photoresist 10a layers are then removed using a conventional method to leave just the patterned hardmask 6 atop the polysilicon target layer 4. As shown in Figure 1, further etching (for example reactive ion etching ( RIE)) is used to etch the complete high resolution pattern to the target layer 4. Once this has been done, the residual hardmask 6 is removed, for example using etching, to yield the final structure shown in Figure lj.
SUMMARY
The process described above may suffer from a patterning error resulting from one or more different components of the lithographic apparatus, including the patterning device, and / or the method by which the pattern is provided in the various layers of material provided on the substrate. The latter issue is related in part to the different topography or the first and second layers of resist and BARC material. While the first pattern is provided in substantially flat, uniform layers of resist and BARC material provided on a substantial flat hardmask layer, the second pattern is provided in second, less uniform, layers of resist and BARC material is deposited on the hardmask layer which now carries the first pattern. Moreover, hi ^ i temperature deposition of the hardmask layer initially can induce stress in the target and / or substrate layers which may then be relieved by partially removing the hardmask during the first patterning step. As a result, the target and / or substrate layers may deform between the first and second patterning steps, which may lead to pattern overlay errors. Difficulties may therefore be encountered in a high resolution patterning procedure, such as the procedure described above, which results in pattern overlay errors and a consistent loss in patterning accuracy and resolution.
There is a desire to use an alternative technique to achieve patterns with increased resolution. To this end, there is a desire to be able to assess the degree to which the lithographic apparatus contributes to patterning errors, which is, as far as possible, independent of the particular patterning process employed.
According to an aspect of the invention, there is provided a method for providing a pattern on a substrate, including method: providing a first pattern in a first layer or photoresist and a first layer or a first bottom anti-reflective coating material on the substrate; etching the first pattern into the substrate; providing a second layer or photoresist and a second layer or a second bottom anti-reflective coating material on the substrate; providing a second pattern in the second layers of photoresist and the second bottom anti-reflective coating material; and etching the second pattern into the substrate, the first and second patterns on the substrate together defining the pattern.
According to a further aspect of the invention, there is provided a method for testing patterning accuracy of a lithographic apparatus, the method including: providing a first pattern in a first layer or photoresist and a first layer or a first bottom anti-reflective coating material on a substrate; etching the first pattern into the substrate; providing a second layer or photoresist and a second layer or a second bottom anti-reflective coating material on the substrate; providing a second pattern in the second layers of photoresist and second bottom anti-reflective coating material; etching the second pattern into the substrate, the first and second patterns to the substrate together defining a test pattern to the substrate; and analyzing the test pattern provided on the substrate to test the patterning accuracy of the lithographic apparatus.
LETTER DESCRIPTION OF THE DRAWINGS
Embodiments of the invention will now be described, by way of example only, with reference to the accompanying schematic drawings in which corresponding reference symbols indicate corresponding parts, and in which: - Figures la to lj show schematically a lithographic method; - Figures 2a to 2k show schematically a lithographic method according to an embodiment of the invention; and - Figure 3 schematically depicts a lithographic apparatus which can be used in a method according to an embodiment of the invention.
DETAILED DESCRIPTION
Figures 2a to 2k show schematically a dual-line, double patterning method for providing a high resolution pattern in a substrate 2, e.g., a silicon substrate. The patterned substrate can be used to test the fidelity or accuracy of the patterning process by subsequent analysis or the final pattern formed in the substrate 2.
Figure 2a shows in cross-section a portion of a substrate 2 provided with a layer of a first bottom anti-reflective coating (BARC) material 8 and photoresist 10. In an embodiment, the BARC material is an organic BARC material and may be any suitable organic BARC material 8 such as, but not limited to, Brewer Science's ARC29 BARC material. The BARC material 8 may be deposited so as to provide a BARC layer 8 or any appropriate thickness, for example the BARC layer 8 may have a thickness or at least around 35 nm, although a thicker layer or BARC material 8 may be provided. The photoresist 10 may be, for example, a positive tone photoresist, although any appropriate type or photoresist can be used. The photoresist 10 may be selected to be sensitive to radiation for an example, 193 nm or 248 run A lithographic apparatus, which may be an example of the type shown schematically in Figure 3, is used to expose a pattern in the photoresist 10. The exposed photoresist 10 is then removed using a developer, such as a caustic solution containing hydroxide ions, so that only unexposed photoresist 10 remains, as shown in Figure 2b.
The pattern is then transferred to the BARC material 8 using an appropriate etching process, such as an ion etch, to provide the structure shown in Figure 2c. The BARC 8 etching process may, for example, employ a plasma including argon, oxygen and chlorine (which may involve a slight over etch of the pattern features to ensure that no material is left in between patterned features that might act as a micro mask during the substrate etch) to both open the BARC layer 8 and trim the patterned features to the desired width. The BARC 8 etching process may be carried out using any convenient instrument, for example, a Hitachi 711M instrument. The pattern formed in the photoresist layer 10 and BARC layer 8 shown in Figure 2c comprises four lines 12 that extend perpendicularly to the plane of Figure 2c. The full width of each line 12 is one-third the width of the space 14 between each pair of lines 12. Only four lines 12 are shown, but it will be appreciated that Figure 2c shows only a portion of the substrate 2, and that many more lines 12 may be provided on the substrate 2.
Referring to Figure 2d, the pattern formed in the photoresist 10 and BARC layer 8 is transferred directly to the substrate 2 using any appropriate silicon etch process, such as reactive ion etching (RIE). The silicon etch process may employ a native oxide etch using a plasma containing chlorine and hydrogen bromide and a plasma containing oxygen, chlorine and hydrogen bromide, although any appropriate plasma may be used. Any convenient instrument may be used to carry out the silicon etching process, e.g., a Hitachi 711M instrument.
The plasma that is present during the silicon etch process generates a polymeric material including photoresist 10, BARC 8 and silicon halogen compounds which are deposited as a protective polymeric layer 16 along the sidewalls of the patterned stacks incorporating layers of photoresist 10, BARC 8 and substrate 2.
The photoresist 10 and BARC 8 layers are removed using any appropriate method, for example a solvent base strip or a sulfuric acid peroxide mixture (SPM) strip. A further example is ashing. One non-limiting example of a suitable ashing process employs a plasma containing oxygen, nitrogen and hydrogen and heating the substrate 2 carrying the patterned photoresist 10 and BARC 8 layers by means of radiation to an elevated temperature, for example a temperature or at least around 200 ° C, or at least around 250 ° C, or or around 270 ° C. Any suitable instrument can be used to carry out the ashing process, e.g. an AXCELIS ES3 instrument. This process does not remove the polymeric sidewall layers 16, which, due to a lack of physical support, collapse towards the exposed uppermost surface of the features formed in the substrate 2, as shown in Figure 2nd, so as to provide further protective polymeric layers 18. Referring to Figure 2f, new layers of a second BARC material 8a and photoresist 10a are provided on the patterned substrate 2 carrying its protective polymeric layers 16.18. Any suitable BARC material 8 may be used, for example, but not limited to, an organic BARC material such as Brewer Science ARC29 BARC. The BARC material 8a may be deposited so as to provide a BARC layer 8a or any appropriate thickness. A desired thickness of the BARC layer 8a depends upon various factors, such as the nature of the photoresist 10a, the substrate 2 and the settings of the lithographic apparatus. The BARC layer 8 may have a thickness or at least around 35 nm. Desirably a thicker layer of BARC material 8a is deposited so as to provide the new layer of BARC material 8a with an upper surface that is as flat as possible and level the topography of the BARC layer 8a, which may contribute to patterning accuracy. For example, the BARC layer 8 may have a thickness of at least around 50 nm, at least around 60 nm or at least around 70 nm. Furthermore, the BARC material 8a may be provided so as to provide a layer of BARC material 8a that is around 40 to 100 nm in thickness, around 55 to 90 nm in thickness, or around 65 to 90 nm in thickness. A desired thickness for the BARC layer 8a is around 85 nm. A second pattern is then formed in the new layers of photoresist 10a (see Figure 2g) and BARC 8a (see Figure 2h), via, for example, exposure of the photoresist 10a, development of the photoresist 10a, and etching of the BARC 8a , to provide a second set of lines 20 in the space 14 between the first set of lines 12, in this way the first and second sets of patterned lines 12, 20 may be considered as being interleaved. The photoresist 10a may be patterned in any convenient way, for example, the same method may be used to form the second pattern as was used to form the first pattern in the photoresist layer 10 described above. The BARC 8 etching process may, by way of example only, employ a plasma including argon, oxygen and chlorine (which may involve a slight over etch of the pattern features to ensure that no material is left in between patterned features that might act as a micro mask during the substrate etch) to both open the BARC layer 8 and trim the patterned features to the desired width. The BARC 8a etching process may be carried out using, for example, a Hitachi 711M instrument. Each second line 20 may be the same width as each first line 12 and each second line 20 may be provided in the center of the space 14 between each pair of first lines 12. In this way, because the spacing 14 between the first lines 12 was three times the width of each first line 12, and three times the width of each second line 20, the first and second lines 12.20 may be equal in width and regularly spaced apart by a distance that is equal to the width or each line 12, 20.
The portions of the existing patterned substrate 2 which are not covered by the patterned photoresist 10a, BARC 8a or polymeric layers 16.18 (as shown in Figure 2h) are then removed directly by any appropriate silicon etch process, such as a RIE employing, for example, a native oxide etch using a plasma containing chlorine and hydrogen bromide and a plasma including oxygen, chlorine and hydrogen bromide, to yield the structure shown in Figure 2i. A Hitachi 711M instrument may be used to carry out the silicon etching process, although any suitable instrument can be used. During the silicon etching process, further layers of polymeric material 22 are formed and deposited on the sidewalls or the second set of patterned stacks, incorporating layers or photoresist 10a, BARC 8a and substrate 2.
The photoresist and BARC layers 10a, 8a are then removed by any convenient means, such as a solvent base strip, a sulfuric acid peroxide mixture (SPM) strip, or ashing. A non-limiting example of a suitable ashing process employs a plasma containing oxygen, nitrogen and hydrogen and heating the substrate 2 carrying the patterned photoresist 10a and BARC 8a layers by means of radiation to an elevated temperature, for example a temperature or at least around 200 ° C, or at least around 250 ° C, or around 270 ° C. A non-limiting example of a suitable instrument that can be used to carry out the ashing process is an AXCELIS ES3 instrument. This ashing process causes regions 24 of the polymeric sidewall layers 22 to collapse onto the substrate 2 features to provide the structure shown in Figure 2j.
The protective polymeric layers 16.22, 24 provided on patterned features of the substrate 2 are then removed to yield the final patterned silicon substrate 2 as shown in Figure 2k. A convenient method for removing the protective polymeric layers 16.22, 24 is a wet strip process, for example a hydrofluoric acid strip process, optionally also employing hydrogen peroxide, which may be carried out using, for example, an FS1 Mercury instrument. The substrate 2 now carries a high resolution test pattern that can be analyzed using any conventional means to determine the resolution of the test pattern and the accuracy of the patterning process. In this way, an embodiment of the invention may be used to determine patterning accuracy and overlay characteristics of the lithographic apparatus and used to calibrate an apparatus for use in a high resolution patterning procedure. A method according to an embodiment of the invention may be obviate or mitigate at least one or more of the disadvantages associated with the process described in relation to Figures la to lj. A method according to an embodiment of the invention removes the need to use a hardmask material which significantly reduces material costs. The complicated, time consuming and costly processes need for pattern and subsequently remove hardmask materials may therefore no longer be required. One or more problems related to over-etching and under-cutting or features during the patterning process may also be removed which avoids the possibility of such reducing patterning fidelity.
An advantage of a method according to an embodiment of the invention is that one or more of the problems discussed above related to stress-induced deformation of the substrate layer between the first and second patterning steps may be reduced because of the removal of the hardmask layer . Done, a method according to an embodiment of the invention allow the contribution to patterning errors associated with the lithographic apparatus to be assessed in the absence of any contribution to such errors from the hardmask, which represents a significant advance on methods employing a hardmask.
Figure 3 schematically depicts a lithographic apparatus which can be used in a method according to a particular embodiment of the invention. The apparatus comprises: an illumination system (illuminator) IL to condition a beam PB or radiation (eg UV radiation or DUV, such as for example generated by an excimer laser operating at a wavelength of 193 nm or 157 nm, or EUV radiation, such generated by laser-fired plasma source operating at 13.6 nm). a support structure (e.g., a mask table) MT to support a patterning device (e.g., a mask) MA and connected to first positioning device PM to accurately position the patterning device with respect to item PL; a substrate table (e.g., a wafer table) WT to hold a substrate (e.g., a photoresist-coated wafer) W and connected to second positioning device P W to accurately position the substrate with respect to item PL; and a projection system (e.g. a refractive projection lens) PL configured to image a pattern beamed to the radiation beam PB by patterning device MA onto a target portion C (e.g. including one or more dies) or the substrate W.
As here depicted, the apparatus is of a transmissive type (e.g., employing a transmissive mask). Alternatively, the apparatus may be of a reflective type (e.g. employing a programmable mirror array or a type as referred to above).
The illuminator IL receives a beam of radiation from a radiation source SO. The source and the lithographic apparatus may be separate entities, for example when the source is an excimer laser. In such cases, the source is not considered to be part of the lithographic apparatus and the radiation beam is passed from the source SO to the illuminator IL with the aid of a beam delivery system BD including for example suitable directing mirrors and / or a beam expander. In other cases the source may be an integral part of the apparatus, for example when the source is a mercury lamp. The source SO and the illuminator IL, together with the beam delivery system BD if required, may be referred to as a radiation system.
The illuminator IL may include adjusting means AM for adjusting the angular intensity distribution of the beam. Generally, at least the outer and / or inner radial extent (commonly referred to as σ-outer and σ-inner, respectively) or the intensity distribution in a pupil plane or the illuminator can be adjusted. In addition, the illuminator IL generally comprises various other components, such as an integrator IN and a condenser CO. The illuminator provides a conditioned beam of radiation PB, having a desired uniformity and intensity distribution in its cross-section.
The radiation beam PB is an incident on the patterning device (e.g., mask) MA, which is a hero on the support structure MT. Having traversed the patterning device MA, the beam PB passes through the projection system PL, which is the beam onto a target portion C or the substrate W. With the aid of the second positioning device PW and position sensor IF (eg an interferometric device) , the substrate table WT can be moved accurately, eg so as to position different target portions C in the path of the beam PB. Similarly, the first positioning device PM and another position sensor (which is not explicitly depicted in Figure 3) can be used to accurately position the patterning device MA with respect to the path of the beam PB, eg after mechanical retrieval from a mask library, or during a scan. In general, movement of the object tables MT and WT will be realized with the aid of a long-stroke module (coarse positioning) and a short-stroke module (fine positioning), which form part of the positioning device PM and PW. However, in the case of a stepper (as opposed to a scanner) the support structure MT may be connected to a short stroke actuator only, or may be fixed. Patterning device MA and substrate May be aligned using patterning device alignment marks M1, M2 and substrate alignment marks P1, P2.
The depicted apparatus can be used in the following preferred modes: 1. In step mode, the support structure MT and the substrate table WT are kept essentially stationary, while an entire pattern is imparted to the beam PB is projected onto a target portion C in one go (ie a single static exposure). The substrate table WT is then shifted in the X and / or Y direction so that a different target portion can be exposed. In step mode, the maximum size of the exposure field limits the size of the target portion C imaged in a single static exposure. 2. In scan mode, the support structure MT and the substrate table WT are scanned synchronously while a pattern is transmitted to the beam PB is projected onto a target portion C (i.e. a single dynamic exposure). The velocity and direction of the substrate table WT relative to the support structure MT is determined by the (de-) magnification and image reversal characteristics of the projection system PL. In scan mode, the maximum size of the exposure field limits the width (in the non-scanning direction) or the target portion in a single dynamic exposure, whereas the length of the scanning motion has the height (in the scanning direction) of the target portion. 3. In another mode, the support structure MT is kept essentially stationary holding a programmable patterning device, and the substrate table WT is moved or scanned while a pattern is imparted to the beam PB is projected onto a target portion C. In this mode, generally a pulsed radiation source is employed and the programmable patterning device is updated as required after each movement of the substrate table WT or in between successive radiation pulses during a scan. This mode of operation can be readily applied to maskless lithography that utilizes programmable patterning device, such as a programmable mirror array or a type as referred to above.
Combinations and / or variations on the modes described above or use or entirely different modes or use may also be employed.
The materials used in the examples described above in relation to Figures 1 and 2 are given as examples only. Other materials may be used. Although the described do not refer to trenches and lines, an embodiment of the invention may be used to form other structures. Although the apparatus and method described above according to an embodiment of the invention are discussed in relation to providing a test pattern in a substrate which can be analyzed to determine patterning overlay errors, it should be appreciated that the patterning method is applicable to patterning a substrate for any desirable purpose and is not necessarily limited to just providing a pattern for purely analytical purposes.
Where specific reference has been made above to use the lithographic apparatus in the manufacture of ICs, but it should be understood that the method described may be applied to the manufacture of integrated optical systems, guidance and detection patterns for magnetic domain memories, liquid-crystal displays (LCDs), thin-film magnetic heads, etc. The skilled artisan will appreciate that, in the context of such alternative applications, any use of the terms "wafer" or "that" may be considered as synonymous with the more general terms "substrate" or "target portion", respectively.
The terms "radiation" and "beam" used include and compass all types of electromagnetic radiation, including ultraviolet (UV) radiation (eg having a wavelength of 365, 248, 193, 157 or 126 nm) and extreme ultra-violet (EUV) radiation (eg having a wavelength in the range of 5-20 nm), as well as particle beams, such as ion beams or electron beams.
The term "patterning device" used should be broadly interpreted as referring to a device that can be used to impart a radiation beam with a pattern in its cross-section such as creating a pattern in a target portion of the substrate. It should be noted that the pattern imparted to the radiation beam may not exactly correspond to the desired pattern in the target portion of the substrate. Generally, the pattern imparted to the radiation beam will correspond to a particular functional layer in a device being created in the target portion, such as an integrated circuit. A patterning device may be transmissive or reflective. Examples of patterning device include masks, programmable mirror arrays, and programmable LCD panels. Masks are well known in lithography, and include mask types such as binary, alternating phase shift, and attenuated phase shift, as well as various hybrid mask types. An example of a programmable mirror array employs a matrix arrangement of small mirrors, each of which can be individually tilted so as to reflect an incoming radiation beam in different directions; in this manner, the reflected beam is patterned. The support structure holds the patterning device. It holds the patterning device in a way depending on the orientation of the patterning device, the design of the lithographic apparatus, and other conditions, such as for example whether or not the patterning device is a hero in a vacuum environment. The support can use mechanical clamping, vacuum, or other clamping techniques, for example electrostatic clamping under vacuum conditions. The support structure may be a frame or table, for example, which may be fixed or movable as required and which may ensure that the patterning device is at a desired position, for example with respect to the projection system. Any use of the terms "reticle" or "mask" may be considered synonymous with the more general term "patterning device".
The term "projection system" used should be broadly interpreted as encompassing various types of projection system, including refractive optical systems, reflective optical systems, and catadioptric optical systems, as appropriate for example for the exposure radiation being used, or for other factors such as the use of an immersion fluid or the use of a vacuum. Any use of the term "projection lens" may also be considered as synonymous with the more general term "projection system".
The illumination system may also encompass various types of optical components, including refractive, reflective, and catadioptric optical components for directing shaping, or controlling the beam of radiation, and such components may also be referred to, collectively or singularly, as a "lens" .
The lithographic apparatus may be of a type having two (dual stage) or more substrate tables (and / or two or more support structures). In such "multiple stage" machines the additional tables and / or support structures may be used in parallel, or preparatory steps may be carried out on one or more tables and / or support structures while one or more other tables and / or support structures are being used for exposure.
The lithographic apparatus may also be of a type bearing the substrate is immersed in a liquid having a relatively high refractive index, e.g. water, so as to fill a space between the final element of the projection system and the substrate. Immersion techniques are well known in the art for increasing the numerical aperture of projection systems.
While specific expired or the invention have been described above, it will be appreciated that the invention may be practiced otherwise than as described. The description is not intended to limit the invention.
Aspects of the invention are as set out in the following, numbered clauses:
CLAUSES 1. A method for providing a pattern on a substrate, including: providing a first pattern in a first layer or photoresist and a first layer or a first bottom anti-reflective coating material on the substrate; etching the first pattern into the substrate; providing a second layer or photoresist and a second layer or a second bottom anti-reflective coating material on the substrate; providing a second pattern in the second layers of photoresist and the second bottom anti-reflective coating material; and etching the second pattern into the substrate, the first and second patterns on the substrate together defining the pattern. 2. The method of clause 1, the first bottom anti-reflective coating material is an organic bottom anti-reflective coating material. 3. The method of clause 1, the second bottom anti-reflective coating material is an organic bottom anti-reflective coating material. 4. The method of any of the clauses 1 to 3, the first pattern and the second pattern are a reactive ion etching. 5. The method of clause 4, the reactive ion etching includes using a plasma including oxygen, chlorine and hydrogen bromide. 6. The method of clause 1, including after the etching the first pattern and before the providing the second layer of photoresist and the second layer of a second bottom anti-reflective coating material, a removing or residual photoresist and residual bottom anti-reflective coating material, from the substrate by ashing. 7. The method of clause 1, including after the etching the second pattern of a removing or residual photoresist and residual bottom anti-reflective coating material from the substrate by ashing. 8. The method of clause 6 or 7, which includes using a plasma. 9. The method of clause 8, comprising the plasma comprises oxygen, nitrogen and hydrogen. 10. The method of clause 6 or 7 according to the ashing comprises heating residual photoresist, or residual bottom anti-reflective coating material, or residual photoresist and the residual bottom anti-reflective coating material, selected from the group consisting of at least around 200 ° C, at least around 250 ° C, and around 270 ° C. 11. The method of clause 6 or 7, further including depositing a layer or polymeric material on the substrate. 12. The method of clause 11, further including removing the layer of polymeric material from the substrate by applying a wet strip after the etching the second pattern into the substrate. 13. The method of clause 12, applying the wet strip comprises applying a hydrofluoric acid stripping process. 14. The method of any of the clauses 1 - 7, the first pattern and the second pattern comprises a series of lines. 15. The method of clause 14, the second pattern is interleaved with the first pattern such that the pattern has a higher resolution than the first pattern or the second pattern. 16. The method of any of the clauses 1 - 7, the substrate comprises a silicon substrate. 17. The method of any of the clauses 1 to 3, the first pattern or the second pattern is a reactive ion etching. 18. The method of any of the clauses 1 to 3, including the first pattern or the second pattern including using a plasma containing oxygen, chlorine and hydrogen bromide. 19. The method of clause 1, including after the etching the first pattern and before the providing the second layer of photoresist and the second layer of a second bottom anti-reflective coating material, a removing or residual photoresist or residual bottom anti-reflective coating material, from the substrate by ashing. 20. A method for testing patterning accuracy or a lithographic apparatus, including: providing a first pattern in a first layer or photoresist and a first layer or a first bottom anti-reflective coating material on a substrate; etching the first pattern into the substrate; providing a second layer or photoresist and a second layer or a second bottom anti-reflective coating material on the substrate; providing a second pattern in the second layers of photoresist and the second bottom anti-reflective coating material; etching the second pattern into the substrate, the first and second patterns to the substrate together defining a test pattern to the substrate; and analyzing the test pattern provided on the substrate to test the patterning accuracy of the lithographic apparatus. 21. The method of clause 20, the first or the second bottom anti-reflective coating material is an organic bottom anti-reflective coating material. 22. The method of clause 20, the first pattern, or the second pattern, or the first and second patterns, is etched into the substrate using reactive ion etching.
权利要求:
Claims (2)
[1]
A method of patterning a substrate, comprising: applying a first pattern to a first layer of photoresist and a first layer of a first bottom anti-reflective coating material on the substrate; etching the first pattern in the substrate; applying a second layer of photoresist and a second layer of a second bottom anti-reflective coating material to the substrate; applying a second pattern in the second layer of photoresist and the second layer of the second bottom anti-reflective coating material; and etching the second pattern in the substrate, the first and second patterns defining the pattern together on the substrate.
[2]
A method of testing a pattern accuracy of a lithographic apparatus, the method comprising: applying a first pattern in a first layer of photoresist and a first layer of a first bottom anti-reflective coating material on the substrate; etching the first pattern in the substrate; applying a second layer of photoresist and a second layer of a second bottom anti-reflective coating material to the substrate; applying a second pattern in the second layer of photoresist and the second layer of the second bottom anti-reflective coating material; and etching the second pattern in the substrate, wherein the first and the second pattern together define a test pattern in the substrate; and analyzing the test pattern applied to the substrate to determine the patterning accuracy of the lithographic apparatus.
类似技术:
公开号 | 公开日 | 专利标题
EP1744211A1|2007-01-17|Substrate, lithographic multiple exposure method, machine readable medium
US7687209B2|2010-03-30|Lithographic apparatus and device manufacturing method with double exposure overlay control
US7781149B2|2010-08-24|Reduced pitch multiple exposure process
US20070190762A1|2007-08-16|Device manufacturing method and computer program product
EP2304504A1|2011-04-06|Overlay measurement apparatus, lithographic apparatus, and device manufacturing method using such overlay measurement apparatus
US8980724B2|2015-03-17|Alignment target contrast in a lithographic double patterning process
US20110273685A1|2011-11-10|Production of an alignment mark
US20050224724A1|2005-10-13|Lithographic apparatus, device manufacturing method and device manufactured thereby
US8119333B2|2012-02-21|Lithographic method
US8252491B2|2012-08-28|Method of forming a marker, substrate having a marker and device manufacturing method
US20060035159A1|2006-02-16|Method of providing alignment marks, method of aligning a substrate, device manufacturing method, computer program, and device
US20080160458A1|2008-07-03|Lithographic device manufacturing method, lithographic cell, and computer program product
US7382438B2|2008-06-03|Lithographic apparatus and device manufacturing method
US8017310B2|2011-09-13|Lithographic method
US7616291B2|2009-11-10|Lithographic processing cell and device manufacturing method
KR20100122441A|2010-11-22|Improving alignment target contrast in a lithographic double patterning process
US20110310369A1|2011-12-22|Lithographic method and apparatus
同族专利:
公开号 | 公开日
US20090148796A1|2009-06-11|
JP2009094481A|2009-04-30|
US8119333B2|2012-02-21|
JP4800354B2|2011-10-26|
引用文献:
公开号 | 申请日 | 公开日 | 申请人 | 专利标题

JP2803999B2|1993-11-10|1998-09-24|現代電子産業株式会社|Method for manufacturing fine pattern of semiconductor device|
KR100223325B1|1995-12-15|1999-10-15|김영환|Method for manufacturing fine pattern of semiconductor device|
AU2300099A|1998-02-09|1999-08-23|Nikon Corporation|Method of adjusting position detector|
JP4251296B2|1998-02-09|2009-04-08|株式会社ニコン|Measurement method, adjustment method, marked object, and detection apparatus|
KR20010004612A|1999-06-29|2001-01-15|김영환|Photo mask and method for forming fine pattern of semiconductor device using the same|
KR100360397B1|1999-11-26|2002-11-18|삼성전자 주식회사|Resist removing composition and resist removing method using the same|
JP2001176788A|1999-12-21|2001-06-29|Hitachi Ltd|Pattern-forming method and semiconductor device|
AT501463T|2001-05-18|2011-03-15|Koninkl Philips Electronics Nv|LITHOGRAPHIC METHOD OF GENERATING AN ELEMENT|
US6680164B2|2001-11-30|2004-01-20|Applied Materials Inc.|Solvent free photoresist strip and residue removal processing for post etching of low-k films|
US7125645B2|2002-04-10|2006-10-24|United Microelectronics Corp.|Composite photoresist for pattern transferring|
JP2004296930A|2003-03-27|2004-10-21|Nec Electronics Corp|Pattern forming method|
US7265056B2|2004-01-09|2007-09-04|Taiwan Semiconductor Manufacturing Company, Ltd.|Method for forming novel BARC open for precision critical dimension control|
US7288484B1|2004-07-13|2007-10-30|Novellus Systems, Inc.|Photoresist strip method for low-k dielectrics|
US7432172B2|2005-01-21|2008-10-07|Tokyo Electron Limited|Plasma etching method|
US20070018286A1|2005-07-14|2007-01-25|Asml Netherlands B.V.|Substrate, lithographic multiple exposure method, machine readable medium|
US7582413B2|2005-09-26|2009-09-01|Asml Netherlands B.V.|Substrate, method of exposing a substrate, machine readable medium|
KR100876808B1|2006-07-10|2009-01-07|주식회사 하이닉스반도체|Method for Pattern Formation of Semiconductor Device|
US20080199814A1|2006-12-06|2008-08-21|Fujifilm Electronic Materials, U.S.A., Inc.|Device manufacturing process utilizing a double patterning process|
KR100886221B1|2007-06-18|2009-02-27|삼성전자주식회사|Method of forming protection layer on the photoresist pattern and method of forming fine pattern using the same|US20090104566A1|2007-10-19|2009-04-23|International Business Machines Corporation|Process of multiple exposures with spin castable film|
US8158334B2|2008-01-14|2012-04-17|International Business Machines Corporation|Methods for forming a composite pattern including printed resolution assist features|
US7883829B2|2008-08-01|2011-02-08|International Business Machines Corporation|Lithography for pitch reduction|
JP2011066120A|2009-09-16|2011-03-31|Toppan Printing Co Ltd|Pattern forming method and pattern form|
US8502324B2|2009-10-19|2013-08-06|Freescale Semiconductor, Inc.|Semiconductor wafer having scribe lane alignment marks for reducing crack propagation|
法律状态:
2009-05-06| AD1A| A request for search or an international type search has been filed|
2009-08-03| EDI| The registered patent application has been withdrawn|
优先权:
申请号 | 申请日 | 专利标题
US93558607P| true| 2007-08-20|2007-08-20|
US93558607|2007-08-20|
[返回顶部]